Most Formnext booths sell a machine. The Fraunhofer ADDITIV stand in Hall 11.0, Booth D31, did something else. It used one aisle to show how far printable materials have moved past the familiar trade-offs of strength, heat and geometry. According to the network's official overview of exhibits at formnext 2026, the institutes brought printed thermal hardware, crack-prone superalloys, ceramics bonded to copper, a shape-memory polymer built for spacecraft, and software that changes how multimaterial prints are planned. 3D Printing Industry's report added preliminary test figures and further detail on several exhibits.
The common thread is function. Most of these parts are not printed because printing is cheaper. They are printed because the internal channels, graded compositions or tuned material behavior they depend on are hard to make any other way.
Heat Is the Headline
The exhibit with the biggest number came from Fraunhofer IWU and Fraunhofer IPM: copper pulsating heat pipes. Fraunhofer describes pulsating heat pipes as passive two-phase heat transport without pumps or moving parts, dissipating heat very effectively while taking up minimal space. In the usual design, working fluid sits in a serpentine channel as alternating slugs of liquid and vapor, and heat at one end drives oscillations that carry energy to the cold end. The channel geometry does the work, and that makes the design a natural fit for additive manufacturing.
According to 3D Printing Industry, the postcard-sized demonstrators are 2.8 mm high and dissipated around 1,200 W in preliminary tests. "Preliminary" matters: treat the figure as a sign of direction rather than a datasheet value. Even so, shedding that much heat through something under 3 mm thick is the kind of result that gets power-electronics engineers to pay attention.
IWU also showed heat exchangers designed by CFD-driven topology optimization using ToffeeX. In Fraunhofer's words, the institute starts with the function itself: cooling structures evolve directly from thermal and fluidic requirements, with material properties and manufacturing constraints considered from the start. That is the opposite of an engineer drawing fins and then checking them in simulation. Fraunhofer IKTS came at cooling from the semiconductor side with an additively manufactured ceramic liquid-cooled heatsink with cooling channels and thick copper layers of 300 micrometres, aimed at bare semiconductor dies and described as a substrate for power electronics. Putting ceramic and a thick copper layer in one printed part is attractive for thermal design, where every interface between materials tends to add resistance.
IKTS also presented diamond composites aimed at applications such as heat exchangers. 3D Printing Industry reports that they offer wear resistance as well as thermal conductivity, and that they can be built in complex geometries.
Materials That Fight Back
Two exhibits dealt with materials that resist conventional laser processing. Fraunhofer IFAM showed sinter-based additive processes for nickel-based superalloys that tend to crack or develop residual stresses under laser-based processing. According to 3D Printing Industry, the sinter route sidesteps those problems, making these alloys accessible to additive manufacturing in ways that laser-based methods have not. It is a useful reminder that some of the most demanding alloys are the ones that melt-based printing handles worst.
Fraunhofer IGCV showed functionally graded tungsten-copper composites designed to withstand extreme conditions in future fusion reactors. Tungsten and copper bring very different properties, and joining dissimilar materials with a sharp interface is a classic source of thermal-stress trouble, so grading the composition across the part is the logical approach. 3D Printing Industry notes that no performance data was provided, so for now this is a capability demonstration rather than a validated component.
Parts That Move Without Mechanisms
The most maker-legible exhibit may be Fraunhofer IAP's shape-memory polymer, which the exhibit list describes as application-specific, qualified for additive manufacturing, and switching at approximately 120 °C. The target is lightweight satellite components; 3D Printing Industry describes additively manufactured hinges for deploying solar panels on satellites. A shape-memory part can be programmed into one shape and then return to another when heated past its switching temperature, which lets a hinge deploy without a separate mechanism.
The same idea of putting behavior into structure shows up in the ProFi finger, described by 3D Printing Industry as a single-piece passive prosthetic finger joint made from a programmable metamaterial with a bistable structure. It replaces several conventional parts. The work came from Fraunhofer's Cluster of Excellence for Programmable Materials (CPM), with IWM, LBF, ITWM and IAP involved. A bistable structure holds more than one stable position, and here that happens without springs, screws or extra joints, so the motion and the holding positions come from the geometry.
Fraunhofer ILT added two functional metal parts. One is a smart wrench with a strain gauge integrated into its metal body during powder bed fusion, so the sensor is built into the tool instead of added afterward. The other is a set of porous titanium LPBF structures for electrolyzer cells, combining water supply, gas removal, electrical conductivity and mechanical stability in one printed component. ILT also showed a large-format optical carrier demonstrator in AlSi10Mg printed by PBF-LB/M, with a sandwich design that combines low mass with the stiffness needed for precise optical alignment. It demonstrates AlSi10Mg processing on the SkalAr concept for build volumes up to 1.0 x 0.8 x 0.4 m.
The Process and Software Layer
Several exhibits focused on how materials are handled and how prints are planned. ILT's patented Fluidic Powder Switch controls powder flow in laser metal deposition and EHLA processes without mechanical wear, and is claimed to be up to 20 times faster than conventional mechanical systems. Fraunhofer IWS's Laser Direct Plating, aimed at coating rotationally symmetric components, is claimed to cut energy consumption by up to 90 percent. 3D Printing Industry describes both as ceiling figures, with actual performance varying with operating conditions. Fraunhofer IWM showed FlowBoard for powder-flow characterization, and the exhibit list also includes CT inspection from IMTE for checking dimensional accuracy and defects.
On the software side, Fraunhofer IGD showed its Cuttlefish multimaterial printer driver, a printer-agnostic tool that controls multimaterial printers at native voxel resolution to reproduce the shape and appearance of a model, including color, translucency and gloss. IGD and IGCV also showed shape dithering, which Fraunhofer describes as a parameter-free geometric method that removes voxel quantization artifacts in 3D printing. Anyone who has looked closely at a sloped surface on a layer-based print knows the stair-stepped look that voxel quantization can produce, and a purely geometric fix is an appealing answer to it.
What It Means for Makers
None of this will turn up in a filament spool next month. Sinter-based superalloys, graded tungsten-copper and ceramic-copper heatsinks are industrial and research work, and several of the headline numbers are preliminary results or best-case claims. The design ideas behind them carry over more readily than the materials do.
The heat-pipe and topology-optimized exchanger work shows how much of thermal design comes down to geometry. Makers working with printing services or their own machines can explore the same principle, at least in prototype form. The shape-memory polymer and the bistable ProFi finger make a lesson familiar from compliant mechanisms concrete: a well-designed structure can replace assemblies of springs, screws and joints. That idea works at the scale of a satellite hinge and, in principle, in PETG on a workbench. Shape dithering is a reminder that some print-quality problems are software problems and can be addressed in the toolchain rather than in the hardware.
The bottom line is that Fraunhofer's Formnext showing suggests the next gains in additive manufacturing may come less from faster machines and more from parts whose materials and geometry do the work. Watch for the heat-pipe figures to firm up with published test conditions, and for performance data on the tungsten-copper work.