In electron-beam powder bed fusion, build temperature has long been something the process imposes on you, not a setting you choose. Wayland Additive, the Huddersfield, England company behind the Calibur3 system, argues that its NeuBeam process changes that. In an interview published by 3D Printing Industry on November 16, 2026, ahead of Formnext, CEO Will Richardson laid out the claim. If you actively neutralise the charge the electron beam leaves in the powder, you no longer have to sinter the whole bed to keep it in place. Once that requirement is gone, temperature becomes a variable you can set for each alloy.

A Semiconductor Answer to a Powder Problem

Wayland's origins explain its approach. Co-founder Ian Laidler had spent decades in the semiconductor industry working on electron-beam lithography at nanometre scales, and he saw a chance to bring that expertise into metal additive manufacturing. Richardson joined him to lead the project. The two began working together in 2016, and NeuBeam is the result of applying that background to metal powder.

The problem they targeted is familiar to anyone who has looked into EB-PBF. An electron beam transfers charge to the powder, which can then scatter inside the machine and disturb the thin, level layer the operator has just laid down. The industry calls this a smoke event. The conventional defence is to heat the powder bed until the particles sinter into a lightly bonded cake, which keeps the powder in place while the beam melts selected areas. That works, but it ties the bed temperature to the need to sinter, and it leaves the finished part encased in that cake. Richardson described holding the bed in a "Goldilocks zone": hot enough to sinter, cool enough for the operator to break the cake away from the part.

Wayland's company site describes NeuBeam as an eBeam metal AM process that effectively neutralises the electron beam in powder bed fusion. It positions the Calibur3 as a compelling alternative to both laser powder bed fusion (L-PBF) and traditional eBeam machines. As described in the interview, active charge neutralisation removes the need to sinter the whole bed. The machine can keep the growing part hot while the surrounding powder stays comparatively loose.

Why Loose Powder Matters

Separating "the part is hot" from "the powder is fused" is the key mechanism, and it has consequences you can see.

The first is depowdering. Richardson used a turbine blade as the example. Certain nickel-based superalloys valued by gas turbine manufacturers are prone to cracking during printing, and a hot build can help. But if powder sinters inside the blade's cooling galleries, the manufacturer inherits a difficult removal job. Richardson said Wayland has cleared channels as small as 1 mm. Internal cooling geometry is one of the main reasons to use additive manufacturing for hot-section components at all, and it only pays off if the powder inside can actually be removed.

The second is temperature freedom. Because bed temperature no longer has to be high enough to sinter everything, it can be chosen to suit the metallurgy of the alloy being printed. Wayland's materials page frames this as superior control over material properties. The interview gives concrete examples at both ends of the range.

Hot for Superalloys

At the high end are nickel superalloys. Richardson singled out CM247 and related high gamma-prime alloys as materials attracting particular interest. These materials are prized for strength at temperature and are prone to cracking during printing. Holding the part hot during the build is the lever here, since a hot build can help. Pairing that with the ability to clear 1 mm cooling channels is clearly aimed at turbine-blade-type parts, which need both the difficult alloy and the internal features.

Advertisement

Titanium: Less Support, Less Post-Processing

For titanium, the benefits Richardson described are mostly geometric and process-related. Thick sections can accumulate residual stress during a build and distort unless substantial supports hold them to the plate. Richardson said Wayland's temperature control allows some such parts to be built with finer, porous supports designed to break away where they meet the component. On suitable jobs, it also allows a thinner substrate and eliminates a separate stress-relief treatment. Still, any reduction in support volume and heat-treatment steps translates into cost and lead time for titanium components.

Cooler for Steels

The less obvious point is that some alloys do better when the process runs cooler. Richardson cited steels whose corrosion resistance suffers at excessive build temperatures. Higher-carbon grades, meanwhile, can reach the required hardness straight off the machine if printed cooler. The saving depends on the customer's specification: a heat treatment can come out of the production route when the as-built part already has the properties that treatment was meant to give it.

Advertisement

This is the core of Wayland's pitch. A process with a fixed thermal profile suits some alloys and fights others. A process where temperature can be dialled in per material can, at least in principle, serve a much wider range of alloys on one machine.

What It Means for Makers

Nobody is putting a Calibur3 in a garage. This is industrial metal AM, aimed at jobs such as turbine-style superalloy parts, titanium components and engineering steels. Richardson himself is candid that electron beam is not for everything: he would leave aluminium to laser powder bed fusion, and sees little reason to switch a thin-walled, lightweight part that already prints reliably on a laser machine. His openings tend to come when a manufacturer faces repeated distortion in a bulky section, an alloy that cracks, or a long wait for a titanium casting.

Still, the underlying lesson will feel familiar to anyone who has tuned a printer: thermal control often decides whether a material prints well or poorly.

What's notable is the claim that charge, not heat, was the real constraint in EB-PBF. Sintering the bed was a workaround for charge management, and the high temperature came along with it. If NeuBeam removes the need for that workaround, temperature is freed to do the metallurgical work engineers actually want it to do. For anyone who ever needs metal parts printed by a service bureau, a mature version of this approach could mean more alloy options, cleaner internal channels and fewer post-processing steps on quotes.

Some caution is warranted. The details here come from the company's own CEO in an interview timed to a trade show, and from Wayland's own marketing. The 1 mm channel result and the alloy-specific benefits are claims worth tracking. Independent part data, qualification results and customer case studies are what will show how far they hold up.

Bottom Line

Wayland Additive's case for NeuBeam is that by neutralising charge in the powder bed, it has turned build temperature from a fixed condition into a design choice. Running hot suits crack-prone alloys like CM247. Running cooler suits steels that would otherwise lose corrosion resistance, and higher-carbon grades that can reach hardness without a separate treatment. Loose powder makes fine internal channels practical to clear. Expect the company to push these points hard at Formnext. The next question is whether production parts confirm them.